nksmfamjp
Well-Known Member
- Joined
- Jan 5, 2004
- Messages
- 3,207
Simply put, I would like to put a SS Barrel on a M70 carbón steel action and have carbon steel NECG sights on the barrel. All coated with Cerakote.....hunting in the rain sometimes.
Will I have galvanic corrosion? Have you tore apart a rifle and seen it? What do people do to prevent it?
Similar question regarding McMillan, B&C or Manners stocks...
Will I have galvanic corrosion? Have you tore apart a rifle and seen it? What do people do to prevent it?
Similar question regarding McMillan, B&C or Manners stocks...