Aluminum Barrel Nut

redneckclimbing

Well-Known Member
Joined
Jan 24, 2012
Messages
303
Has anyone tried an aluminum barrel nut before. I am wanting to build an ULTRA light .260 rem on a rem 700 SA.

Before anyone says, "There are a lot of other places to save weight." Let's just assume that I have taken those into account and OUNCES matter on this build.

Can anyone think of a reason that this will not work?
 
Has anyone tried an aluminum barrel nut before. I am wanting to build an ULTRA light .260 rem on a rem 700 SA.

Before anyone says, "There are a lot of other places to save weight." Let's just assume that I have taken those into account and OUNCES matter on this build.

Can anyone think of a reason that this will not work?



There is no problem if it is the thread protector that replaces the muzzle break.

I would recommend the 7071 grade of aluminum for strength.

J E CUSTOM
 
There is no problem if it is the thread protector that replaces the muzzle break.

I would recommend the 7071 grade of aluminum for strength.

J E CUSTOM


J E-

It will be the barrel nut that holds the barrel in place. Do you see any problems with that? I was thinking the same as fas as material, 7071 T6 Al.
 
Since it only acts as a jam nut it should work, but it may not too. AR's use em' and although not the same design, it's essentially the same thing.
 
J E-

It will be the barrel nut that holds the barrel in place. Do you see any problems with that? I was thinking the same as fas as material, 7071 T6 Al.



I think I would use stainless or Chrome Moly for the barrel nut because of the thread strength and the same coefficient of expansion as the barrel and the action. (Heating and cooling could cause the
nut to loosen)

There are less critical areas to shed weight (Scopes weigh 1 and 1/2 to 3 pounds difference and would be a better place to save weight IMO.

Just my opinion. Better to be safe than sorry.

J E CUSTOM
 
I think I would use stainless or Chrome Moly for the barrel nut because of the thread strength and the same coefficient of expansion as the barrel and the action. (Heating and cooling could cause the
nut to loosen)

There are less critical areas to shed weight (Scopes weigh 1 and 1/2 to 3 pounds difference and would be a better place to save weight IMO.

Just my opinion. Better to be safe than sorry.

J E CUSTOM

J E,

You are spot on but too soft in your words. It's flat a bad idea!

The temperature coefficient difference between barrel/action and nut is significant.

Why would one want to barrel nut a Rem action anyway? If a switch bbl setup is the goal, I see no problem with going nut less. The bbl doesn't have to be "that" tight. Use your personal definition of "that"...
 
An Aluminium barrel nut could work very well or very poorly.
The devil is in the details.
You would need to show a dimensioned sketch.

Here are 3 examples of simple sketches.
 

Attachments

  • Rem700 rebarreling drawing.jpg
    Rem700 rebarreling drawing.jpg
    50 KB · Views: 102
  • Mosin Nagant drawing relieve stock for pillars and Timney trigger and relieve pillar for trigger.jpg
    Mosin Nagant drawing relieve stock for pillars and Timney trigger and relieve pillar for trigger.jpg
    138.6 KB · Views: 116
  • Colt Officers model 22 scope mount bushnell phantom as built drawing gamma 4-10-2013.jpg
    Colt Officers model 22 scope mount bushnell phantom as built drawing gamma 4-10-2013.jpg
    47.9 KB · Views: 111
J E,

You are spot on but too soft in your words. It's flat a bad idea!

The temperature coefficient difference between barrel/action and nut is significant.

Why would one want to barrel nut a Rem action anyway? If a switch bbl setup is the goal, I see no problem with going nut less. The bbl doesn't have to be "that" tight. Use your personal definition of "that"...


The main reason for barrel nutting a Rem is to loose weight in the barrel and still maintain a descent muzzle diameter.

For example a "light Palma" contour barrel will have a shank that is approx. 1.2" for three inches. Instead of with the barrel nut just 1.06 for that same three inches and then tapering from there. Saving you a few ounces with out giving up muzzle diameter.

The coefficeint of thermal expansion with steel and AL are quite different although these numbers are based on the temperature of the metal itself. With the steel being heated from the inside out and and that heat being disappated through the rest of the barrel and receiver steel. Within resonable proximity. Then heating the Al at any given time the temperature of the Al is going to be less. Also Al looses heat faster helping it to maintain a cooler temperature.

I would have to do the numbers to be sure but I would think that they would almost remain at their ambient temperature dimensions even with some fairly extended firing.

JE-

Thinking about it a little more you could be right. You would probably only save at most an ounce (just guessing) and maybe that wouldn't be worth it. I am going to barrel nut this next Rem regardless. So, if I have time maybe I will make an Al nut and let everyone know it works.

P.S. Has anyone actually done this before?
 
Just a thought here, feel free to tell me if I'm off but
why not go with titanium.
 
The expansion of Aluminium is 12.3 10-6 in/in oF
The expansion of steel is 7.3 10-6 in/in oF

If I am doing this right, to get 1% difference in expansion, we would need to change the temp 2000 oF.
 
I believe those are linear expansion numbers but, you do make a point. Stuff really has to heat up to grow enough to get loose. That, combined with it just being a jam nut, makes me think it would work.

Ti would be a very strong option except that it is heavier than Al and is especially hard to machine, (from what I've heard).

With an Al nut 1.30" in diameter and an internal diameter of 1.0" and being .75" long you would save 2.3 oz over a steel barrel nut of the same dimensions.

So, if you barrel nut a Rem action as disucssed earlier you only save about 1.2 oz. with a steel barrel nut. However, with the Al nut you would save about 3.5 oz.

Some people might say that's not worth it but if you figure that a pair of two piece Talley bases weigh about 2 ozs., that might make you think.
 
Trying to organize a group of engineers, I told them that area savings on a military printed wiring board was worth $10 parts price difference per square inch, except along a heat sink where we would give $100.

Likewise on the rifle weight savings, an Aluminium PAWS trigger guard saved weight at a cost of $10 per ounce over the stock steel part
P.A.W.S. at Brownells
 
I believe those are linear expansion numbers but, you do make a point. Stuff really has to heat up to grow enough to get loose. That, combined with it just being a jam nut, makes me think it would work.

Ti would be a very strong option except that it is heavier than Al and is especially hard to machine, (from what I've heard).

With an Al nut 1.30" in diameter and an internal diameter of 1.0" and being .75" long you would save 2.3 oz over a steel barrel nut of the same dimensions.

So, if you barrel nut a Rem action as discussed earlier you only save about 1.2 oz. with a steel barrel nut. However, with the Al nut you would save about 3.5 oz.

Some people might say that's not worth it but if you figure that a pair of two piece Talley bases weigh about 2 ozs., that might make you think.



Thinking outside of the box is always good if you have a single objective in mind (Weight for
example). It breeds innovation but it can also just be a bad idea.

A ultra light rifle has many attributes for carrying and short distance hunting, But from a accuracy
point they are more difficult for the marksman to use at extended distances. (Not as steady and
much more finicky in load development) they can be very accurate under perfect conditions and
positions, (But how often are perfect conditions present while hunting).

Dissimilar metals have a way of causing problems and mixing Aluminum and steel is problematic
and may cause problems. (I once had a 30/378 built on a chrome Molly action, I decided to replace
the action screws with stainless because the factory ones were slot head screws and harder to
torque than the Allen head screws I had.)

Every 8 to 10 shots accuracy would fall off and after checking the torque the screws had loosened.
not believing that the problem was stainless to chrome Molly, I switched back to the steel slot
head screws, end of problem. Later I found some Allen head screws in steel and they are still on
the rifle.

I also don't like the aluminum scope bases and rings because of there strength.Almost without
exception, every failure has been while hunting and I just don't take the chance any more.

I seem to learn my lessons the hard way so I have become very conservative.

Just some recommendations.

J E CUSTOM
 
Warning! This thread is more than 11 years ago old.