Forums
New posts
Search forums
What's new
Articles
Latest reviews
Author list
Classifieds
Log in
Register
What's new
Search
Search
Search titles and first posts only
Search titles only
By:
New posts
Search forums
Menu
Log in
Register
Install the app
Install
Forums
Rifles, Reloading, Optics, Equipment
Gunsmithing
Recoil Bedding; Attempt on HMR
JavaScript is disabled. For a better experience, please enable JavaScript in your browser before proceeding.
You are using an out of date browser. It may not display this or other websites correctly.
You should upgrade or use an
alternative browser
.
Reply to thread
Message
<blockquote data-quote="nksmfamjp" data-source="post: 2704519" data-attributes="member: 1951"><p>I can't tell what im looking at exactly. It looks like you didn't have enough bedding compound, pulled it too early, not enough hardener, something. I think you could possibly use sizing wax, but it seems like drying wax would be much better.</p><p></p><p>Trying to keep bedding in a tiny spot seems like a good idea, but it is probably better to bed the whole thing and clean up afterwards. It is a big job, but worth it.</p></blockquote><p></p>
[QUOTE="nksmfamjp, post: 2704519, member: 1951"] I can‘t tell what im looking at exactly. It looks like you didn’t have enough bedding compound, pulled it too early, not enough hardener, something. I think you could possibly use sizing wax, but it seems like drying wax would be much better. Trying to keep bedding in a tiny spot seems like a good idea, but it is probably better to bed the whole thing and clean up afterwards. It is a big job, but worth it. [/QUOTE]