Forums
New posts
Search forums
What's new
Articles
Latest reviews
Author list
Classifieds
Log in
Register
What's new
Search
Search
Search titles and first posts only
Search titles only
By:
New posts
Search forums
Menu
Log in
Register
Install the app
Install
Forums
Rifles, Reloading, Optics, Equipment
Reloading
Wet tumbling brass - why is my brass getting tarnished?!
JavaScript is disabled. For a better experience, please enable JavaScript in your browser before proceeding.
You are using an out of date browser. It may not display this or other websites correctly.
You should upgrade or use an
alternative browser
.
Reply to thread
Message
<blockquote data-quote="planetwaves" data-source="post: 1577735" data-attributes="member: 84697"><p>I use Frankford Arsenal Brass Cleaning Solution. My tumbler has a 7 liter (7.4 quart) capacity and the instructions call for 4 cap fulls of the solution (a smaller tumbler would use proportionally less). After tumbling for up to two hours, drain out the dirty water and rinse thoroughly to remove solution and dirt inside and outside of cases (there are various ways of doing this). Note: I just use tap water for the entire process and have had no issues with tarnishing, etc. Then drain the water from cases and dry. I use a cookie sheet in the oven at 200 degrees for an hour. Brass comes out looking like new. Although steel pin media came with my tumbler, I have never used it. Once through the above process has been adequate.</p></blockquote><p></p>
[QUOTE="planetwaves, post: 1577735, member: 84697"] I use Frankford Arsenal Brass Cleaning Solution. My tumbler has a 7 liter (7.4 quart) capacity and the instructions call for 4 cap fulls of the solution (a smaller tumbler would use proportionally less). After tumbling for up to two hours, drain out the dirty water and rinse thoroughly to remove solution and dirt inside and outside of cases (there are various ways of doing this). Note: I just use tap water for the entire process and have had no issues with tarnishing, etc. Then drain the water from cases and dry. I use a cookie sheet in the oven at 200 degrees for an hour. Brass comes out looking like new. Although steel pin media came with my tumbler, I have never used it. Once through the above process has been adequate. [/QUOTE]