Forums
New posts
Search forums
What's new
Articles
Latest reviews
Author list
Classifieds
Log in
Register
What's new
Search
Search
Search titles and first posts only
Search titles only
By:
New posts
Search forums
Menu
Log in
Register
Install the app
Install
Forums
Hunting
Long Range Hunting & Shooting
Slick Bolt Parts
JavaScript is disabled. For a better experience, please enable JavaScript in your browser before proceeding.
You are using an out of date browser. It may not display this or other websites correctly.
You should upgrade or use an
alternative browser
.
Reply to thread
Message
<blockquote data-quote="Joel Russo" data-source="post: 1326268" data-attributes="member: 6152"><p>The C12 process gives us a micro-hardness of 1000-2000HV, a build up of only 1.0-5.0 microns, a coefficient of friction of 0.1, and only requires a process temperature of 320* Fahrenheit. </p><p></p><p>I don't know the comparative numbers for melonite off the top of my head, but the DLC treatment kicks the pants off it. Particularly with the low process temperature for DLC.</p></blockquote><p></p>
[QUOTE="Joel Russo, post: 1326268, member: 6152"] The C12 process gives us a micro-hardness of 1000-2000HV, a build up of only 1.0-5.0 microns, a coefficient of friction of 0.1, and only requires a process temperature of 320* Fahrenheit. I don't know the comparative numbers for melonite off the top of my head, but the DLC treatment kicks the pants off it. Particularly with the low process temperature for DLC. [/QUOTE]