Sherman Wildcat Reloading Data is Here!!!

300 Sherman

Fed 210gmm primers; Peterson 280 AI brass (72 gr h20 estimated); H4831SC 57.6; Berger #30414 190 VLD Seated 0.010" into lands(CBTO = 2.730")

Brass prep: Expand to 8mm...two steps; Size to close bolt with light force...my CBTD was like 2.123", but fired case are more like 2.159"...maybe the false shoulder is not required.

Long term, I'm guessing I can run this at like 65000 psi with formed brass, right? I need to develop that load next.

Kind of weird quoting myself, but wanted the data with this…..
Fireformed from my Brux 1:10 twist, this load gave multiple 0.25" 5 shot groups at 100 yds and 2640fps. Great fireforming load! It does flatten primers, even with a good false shoulder. After firing, primers are backed out 0.001", but pretty flat.

Then for my hunting load:

Fed 210gmm primers; Peterson 280 AI brass (72 gr h20 estimated); R26 66.8; Berger 180 EOL Seated 0.050" of lands(CBTO = 2.675") 3057fps

Sd = 8 for 5rds and accuracy is 0.763"…..I need to keep working on seating depth….would like to get under 0.5", but, may just call it for now and work on the shooter! I kind of think I pulled shot #4 there….not sure.
 

Attachments

  • 7DAED9FA-D61D-4AE9-8C6D-95D7636F53A3.jpeg
    7DAED9FA-D61D-4AE9-8C6D-95D7636F53A3.jpeg
    112.6 KB · Views: 71
  • 786AACCB-1824-4C13-86CF-B39D2306187C.jpeg
    786AACCB-1824-4C13-86CF-B39D2306187C.jpeg
    390.7 KB · Views: 71
I've been working on a couple different loads for the 7 Max. All loads are built on ADG brass from Rich, Fed 215 primers, and crimped with a Lee FCD. Here's what I've got so far:

Hammer Hunter 131 grain - 2.945 COAL, 70.7 grains of H4831 SC produced 3,545 FPS with an SD of 6.4, and grouped sub 1/4 MOA.

Berger 180 VLD - 3.157 COAL, 66.2 grains H1000 produced 2,992 FPS with an SD of 7.3 and grouped sub 1/2 MOA.

Berger 195 EOL - 3.10 COAL, 68.5 grains N570 produced 2,925 FPS with an SD of 4.7 and grouped a little under 0.3 MOA.

34D5A0D5-6862-475F-8C32-FB201E77821E.jpegB2AD7F8B-21E1-4904-B3B1-BFD5BA9FDD99.jpeg55DEB7EF-3684-4017-ACEB-609CFD0AF266.jpeg
 
I've been working on a couple different loads for the 7 Max. All loads are built on ADG brass from Rich, Fed 215 primers, and crimped with a Lee FCD. Here's what I've got so far:

Hammer Hunter 131 grain - 2.945 COAL, 70.7 grains of H4831 SC produced 3,545 FPS with an SD of 6.4, and grouped sub 1/4 MOA.

Berger 180 VLD - 3.157 COAL, 66.2 grains H1000 produced 2,992 FPS with an SD of 7.3 and grouped sub 1/2 MOA.

Berger 195 EOL - 3.10 COAL, 68.5 grains N570 produced 2,925 FPS with an SD of 4.7 and grouped a little under 0.3 MOA.

View attachment 292789View attachment 292790View attachment 292791
three good loads right there!
 